MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akrotek® PK-HM GF 30 (4709) PK Conditioned, 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: The renaissance of this polymer came about with an environmental program aimed at reducing greenhouse gases. The comonomer is CO (carbon monoxide), an industrial „waste” gas, which forms an unusual product when bonding with the polymer. The terpolymer, which forms the basis of most AKROTEK® PK formulations when using the monomers ethylene and propylene, currently has the greatest significance. AKRO-PLASTIC GmbH produces two product families from this base polymer (HM = normal flow and VM = very easy-flowing), based on the former portfolio of the Shell AG, from non-reinforced to high-glass-fibre-reinforced standards, from flame-retardant to carbon-fibre-reinforced custom grades

The characteristic properties of these properties include:

  • excellent dynamic resilience
  • good barrier properties
  • good tribological properties
  • high resistance to chemicals
  • good hydrolysis resistance
  • shorter cycle times
Application areas:
  • Industry
  • Automotive industry
  • Electronics/Electrical

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Filler Content 30 %ISO 1172
Moisture Absorption 0.60 - 0.70 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa5 [mm/min]; ISO 527-2
Elongation at Break >= 3.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 7100 MPa1 [mm/min]; ISO 527-2
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Polygon Composites Polylube® MRP Versatile high load, low friction composite bearings
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
MTI ThermoStran® PPA-50G Long Glass Fiber Compound

PAKRO140 / 182727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.