MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MTI ThermoStran® PPA-50G Long Glass Fiber Compound
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent to the pellet length. Fiber / pellet length = 0.5 inches. Properties reported are dry as molded.

Processing information:

Mold Temperature: Higher mold temperatures are recommended for smoother surface appearance.
Nozzle: Shortest length possible and 0.25 inch diameter or larger is recommended.
Gates: Gates should be as large as possible and located to eliminate knit line and advantageously align fiber.
Runners: Full round runners with 0.25 inch diameter and no sharp corners.
Construction Material: Tool steels can be heat treated and polished to increase hardness and wear resistance. A-2 and D-2 steels can be hardened to Rockwell 60 C scale for longer life.
Plating: Electroless nickel plating may offer additional wear protection.

Information provided by MTI Thermoplastic Composites, Division of Montsinger Technologies, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.59 g/cc1.59 g/cc
Filler Content 50 %50 %Long Glass Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 255 MPa37000 psi
Tensile Modulus 18.6 GPa2700 ksi
Flexural Strength 400 MPa58000 psi
Flexural Modulus 16.5 GPa2400 ksi
Izod Impact, Notched 4.97 J/cm9.30 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 284 °C543 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 321 °C610 °F
Middle Barrel Temperature 329 °C625 °F
Front Barrel Temperature 338 °C640 °F
Nozzle Temperature 338 °C640 °F
Melt Temperature 332 - 349 °C630 - 660 °F
Mold Temperature 135 °C275 °F
Drying Temperature 98.9 °C210 °F
Dry Time 4 hour4 hour
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 MPa12000 psi
Screw Speed 50 - 75 rpm50 - 75 rpm
 
Descriptive Properties
Nozzle ID0.25 Inches
Screw Design20:1 L/D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
Avient Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
RTP Company RTP 4009 MS 2  Polyphthalamide (PPA) Glass Fiber 50% - Molybdenum Disulfide 2%

PMTIG06 / 53900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.