MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shandong Dongyue Shenzhou New Material Co CHFM 300 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Conformable with: Q/DYS 013-2007

Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. The former is for fuel cell membrane and as conductive film for many other usages, the latter for membrane with ion selectivity of chlor-alkali electrolysis tank.

Main Applications:

Mainly for ion membrane caustic soda, hydrogen-oxygen fuel cells, electrodialysis, desalination, water electrolysis.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.93 - 2.03 g/cc0.0697 - 0.0733 lb/in³Resin
Thickness 300 microns11.8 mil
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature >= 350 °C>= 662 °F
 
Descriptive Properties
AppearanceTranslucent membrane
Exchange Capacity (IEC) (mmol/g)0.8-1.15
Group FormulaRf-SO2F, RF-SO3Na, Rf-SO3H

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin
Shandong Dongyue Polymer DF-21B PTFE Presintered Resin
Shandong Dongyue Shenzhou New Material Co CHFM 025 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Shandong Dongyue Shenzhou New Material Co CHF085 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Shandong Dongyue Shenzhou New Material Co CHF080 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)

PSHEN021 / 104076

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.