MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shandong Dongyue Polymer DF-21B PTFE Presintered Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.

Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.

Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.

Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.

Conformable with Q/DYG 007-2004

Information provided by Shandong Dongyue Polymer Material Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Particle Size <= 500 µm<= 500 µm
 
Thermal PropertiesMetricEnglishComments
Melting Point 322 - 332 °C612 - 630 °F
 
Descriptive Properties
Machining MethodRam extrusion
Powder Flow (g/min)450
Smoothness & CleanlinessFirst Grade: Clean and white surface, no metal impurity, the impurity quantity from 1-3 mm doesn't exceed two
 Qualified: Clean and white surface, no metal impurity, the impurity quantity from 1-3 mm doesn't exceed four

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin
Shandong Dongyue Polymer DF-21 PTFE Presintered Resin
Shandong Dongyue Shenzhou New Material Co CHFM 300 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)

PSHADP16 / 103667

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.