MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Magnadie™ Modified H-13 Hot Work Die Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Air-Hardening Steel; Hot Work Steel

Material Notes: MAGNADIE is an AOD refined, air hardenable 5% chromium die steel. It is a good choice for both hot and cold work applications. Magnadie steel possesses improved toughness as compared to standard H-13 while maintaining comparable elevated temperature hardness and strength characteristics. It is also easily machined as it can be annealed to a hardness of approximately 200 BHN. Some typical hot work applications for Magnadie steel include dummy blocks and mandrels for brass and aluminum extrusion, extrusion dies for aluminum and magnesium, hot press dies, punches and dies for shell piercing, die inserts for forging dies, knock out pins, heavy duty shears, slitters and other applications requiring maximum toughness.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 39.6 - 48
Tensile Strength, Ultimate 190.2 - 246.2 ksi
Tensile Strength, Yield 1091 - 1416 MPa
Elongation at Break 12.5 - 14 %
Reduction of Area 36.4 - 38.4 %
Charpy Impact 7.86 - 12.88 JV-Notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.88 µm/m-°C
@Temperature 27.0 - 204 °C
 13.38 µm/m-°C
@Temperature 27.0 - 649 °C
Thermal Conductivity 25.55 W/m-K
@Temperature 20.0 °C
 27.1 W/m-K
@Temperature 649 °C
 28.11 W/m-K
@Temperature 204 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.37 %
Chromium, Cr 5.3 %
Iron, Fe 91.2 %
Manganese, Mn 0.40 %
Molybdenum, Mo 1.35 %
Silicon, Si 1.0 %
Vanadium, V 0.38 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
Assab Steels 8407 SUPREME Hot Work Steel
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.25 in. round High Strength Alloy Steel

NTIMK087 / 19434

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.