MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Latrobe Magnadie™ Modified H-13 Hot Work Die Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Air-Hardening Steel; Hot Work Steel

Material Notes: MAGNADIE is an AOD refined, air hardenable 5% chromium die steel. It is a good choice for both hot and cold work applications. Magnadie steel possesses improved toughness as compared to standard H-13 while maintaining comparable elevated temperature hardness and strength characteristics. It is also easily machined as it can be annealed to a hardness of approximately 200 BHN. Some typical hot work applications for Magnadie steel include dummy blocks and mandrels for brass and aluminum extrusion, extrusion dies for aluminum and magnesium, hot press dies, punches and dies for shell piercing, die inserts for forging dies, knock out pins, heavy duty shears, slitters and other applications requiring maximum toughness.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 39.6 - 4839.6 - 48
Tensile Strength, Ultimate 1311 - 1697 MPa190200 - 246200 psi
Tensile Strength, Yield 1091 - 1416 MPa158200 - 205400 psi
Elongation at Break 12.5 - 14 %12.5 - 14 %
Reduction of Area 36.4 - 38.4 %36.4 - 38.4 %
Charpy Impact 7.86 - 12.88 J5.80 - 9.500 ft-lbV-Notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.88 µm/m-°C
@Temperature 27.0 - 204 °C
6.600 µin/in-°F
@Temperature 80.6 - 399 °F
 13.38 µm/m-°C
@Temperature 27.0 - 649 °C
7.433 µin/in-°F
@Temperature 80.6 - 1200 °F
Thermal Conductivity  25.55 W/m-K
@Temperature 20.0 °C
177.3 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 27.1 W/m-K
@Temperature 649 °C
188 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 28.11 W/m-K
@Temperature 204 °C
195.1 BTU-in/hr-ft²-°F
@Temperature 399 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.37 %0.37 %
Chromium, Cr 5.3 %5.3 %
Iron, Fe 91.2 %91.2 %
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 1.35 %1.35 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 0.38 %0.38 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
Assab Steels 8407 SUPREME Hot Work Steel
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.25 in. round High Strength Alloy Steel

NTIMK087 / 19434

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.