MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inovyn 172GA Polyvinyl Chloride Emulsion Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: Made by emulsion polymerization.

APPLICATIONS
Calendering :
plasticized films and sheets
Extrusion : rigid or plasticized pipes and profiles
In most cases, SolVin 172GA resin is used in blends with suspension resins

Information provided by SolVin.

SolVin is a predecessor company to Inovyn.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content <= 0.30 g/lISO 1269
Apparent Bulk Density 0.660 g/ccISO 1068
Particle Size 63 µm>30% greater than value; ISO 1624
 125 µm<10 g/kg greater than value; ISO 1624
Viscosity Test 132 cm³/gReduced viscosity, K value = 72; ISO 1628-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SABIC PVC 701E Emulsion Polyvinyl Chloride for Paste Preparation
Inovyn 173GB Polyvinyl Chloride Emulsion Polymer
Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)
Teknor Apex APEX® 94-A0098C-90 Polyvinyl Chloride, Flexible
AlphaGary GW 2052 SPECIAL LCF Flame Retardant Polyvinyl Chloride

PSOLVI51 / 68411

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.