Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness. Features: Good or high flow. 40% glass reinforced. Flame retardant. Processing: Injection molding. Former DSM Engineering Plastics product line is now with Envalior. |