MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Xytron™ G4010T PPS-GF40 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.

Features: Good or high flow. 40% glass reinforced. Flame retardant. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Moisture Absorption 0.0400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ISO 2039-2
Hardness, Shore M 100ISO 2039-2
Tensile Strength at Break 55.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 73.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 105 MPa
@Temperature 120 °C
ISO 527-1/-2
 200 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Elongation at Break 2.0 %
@Temperature 23.0 °C
ISO 527-1/-2
 3.1 %
@Temperature 120 °C
ISO 527-1/-2
 3.9 %
@Temperature 160 °C
ISO 527-1/-2
 6.4 %
@Temperature 200 °C
ISO 527-1/-2
Tensile Modulus 3400 MPa
@Temperature 200 °C
ISO 527-1/-2
 5200 MPa
@Temperature 160 °C
ISO 527-1/-2
 7300 MPa
@Temperature 120 °C
ISO 527-1/-2
 15000 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Flexural Strength 300 MPaISO 178
Flexural Modulus 4200 MPa
@Temperature 200 °C
ISO 178
 5000 MPa
@Temperature 160 °C
ISO 178
 10000 MPa
@Temperature 120 °C
ISO 178
 14500 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 10.5 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 56.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 57.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Dielectric Constant 4.0
@Frequency 5.00e+9 Hz
IEC 60250
Dielectric Strength 31.0 kV/mmIEC 60243-1
Dissipation Factor 0.0055
@Frequency 5.00e+9 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°CISO 11359-1/-2
 110 µm/m-°Cabove Tg; ISO 11359-1/-2
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-1/-2
 15.0 µm/m-°Cabove Tg; ISO 11359-1/-2
Melting Point 280 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 265 °CISO 75-1/-2
UL RTI, Electrical 130 °C
@Thickness 0.800 mm
UL746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7951 / 291387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.