MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman Matrixx 55N5006 Flame Retardant Polycarbonate (5VA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Data provided by The Matrixx Group, now a part of A. Schulman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmMatrixx Internal Test
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8800 psi0.125 in; ASTM D638
Flexural Modulus 325000 psiTangent, 0.125 in; ASTM D790
Izod Impact, Notched 13.0 ft-lb/in0.125 in, 73°F; ASTM D256
Gardner Impact >= 320 in-lb
@Temperature 23.0 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 115 °CRelative Thermal Index; UL746
Deflection Temperature at 0.46 MPa (66 psi) 265 °F0.125 in; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °F0.125 in; ASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 3.00 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos L12Z-01 Polypropylene Impact Copolymer
LG Chemical AF-325 ABS Resin
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release
Covestro Makrolon® FR 7087 Polycarbonate
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade

PMAT77 / 52462

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.