MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: ROHS Compliant.

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Water Absorption 0.18 %0.18 %24 hours at 73°F; ASTM D570
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
15 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 58.6 MPa
@Thickness 3.17 mm
8500 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 75 %
@Thickness 3.17 mm
75 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 86.2 MPa
@Thickness 3.17 mm
12500 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.14 GPa
@Thickness 3.17 mm
310 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 5.87 J/cm
@Thickness 3.17 mm
11.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 443 kJ/m²
@Thickness 3.17 mm
211 ft-lb/in²
@Thickness 0.125 in
ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+15 ohm-cm3.00e+15 ohm-cm96 hours at 90°C, 50% RH; ASTM D257
 6.00e+15 ohm-cm6.00e+15 ohm-cm40 hours at 23°C, 50% RH; ASTM D257
Dielectric Strength 24.0 kV/mm
@Thickness 3.17 mm
610 kV/in
@Thickness 0.125 in
ASTM D149
Arc Resistance 60 - 120 sec60 - 120 secPLC 6
Comparative Tracking Index 250 - 400 V250 - 400 VPLC 2
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness 1.50 mm
15 - 30 sec
@Thickness 0.0591 in
PLC 3
 15 - 30 sec
@Thickness 2.50 mm
15 - 30 sec
@Thickness 0.0984 in
PLC 3
 30 - 60 sec
@Thickness 3.00 mm
30 - 60 sec
@Thickness 0.118 in
PLC 2
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 2.50 mm
60 - 120 arcs
@Thickness 0.0984 in
PLC 1
 60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
PLC 1
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
PLC 0
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.2 µm/m-°C
@Temperature -40.0 - 95.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831-06
CTE, linear, Transverse to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831-06
Deflection Temperature at 0.46 MPa (66 psi) 134 °C273 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FASTM D648
UL RTI, Electrical 125 °C257 °F
UL RTI, Mechanical with Impact 115 °C239 °F
UL RTI, Mechanical without Impact 125 °C257 °F
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in
Black, Gray, Beige
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Oxygen Index 37.6 %37.6 %ASTM D2863
Glow Wire Ignition Temperature 775 °C1430 °F
Glow Wire Flammability Index 960 °C1760 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 - 274 °C490 - 525 °F
Middle Barrel Temperature 266 - 277 °C510 - 530 °F
Front Barrel Temperature 277 - 293 °C530 - 560 °F
Nozzle Temperature 271 - 293 °C520 - 560 °F
Melt Temperature 282 - 304 °C540 - 580 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Injection Pressure 75.8 - 124 MPa11000 - 18000 psi
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
 
Descriptive Properties
Edge GateSlow to Medium
Tab GateMedium to Fast
Tunnel GateFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release
PTS Tristar® PC-10FRN-HC Flame Retardant Polycarbonate
LNP Lexan® LF1000N Polycarbonate, 10% PTFE Lubricant
Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized

PZ9PT92V / 21529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.