MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cossa Polimeri ESTABIO PL 0560 T10 Biodegradable Plastic  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: Biodegradable plastic for the extrusion of disposables

Certified for food contact

Information provided by Cossa Polimeri S.r.l.

Key Words: EN 13432
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D 792
Melt Flow <= 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 30 %>= 30 %ASTM D 638
Flexural Modulus 2.80 GPa406 ksiASTM D 790
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inASTM D 256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °F120°C/hr; ASTM D 648
 
Processing PropertiesMetricEnglishComments
Dry Time 3.00 hour
@Temperature 50.0 °C
3.00 hour
@Temperature 122 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ecoflex® 1200 F Blend Biodegradable Polyester
CENTROPLAST BC Organic Thermoplastic
LyondellBasell Hostacom™ RE-44AC Thermoplastic Polyolefin Elastomer
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade

PCOSSA913 / 156503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.