MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Hostacom™ RE-44AC Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hostacom™ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic olefin (TPO) resin. It has an excellent balance of properties and is designed primarily for injection molding applications. This resin is available in black only. It is not intended for food contact applications. Uses: Appliances, automotive applications, lawn and garden equipment

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 17.0 MPa2470 psiISO 527-1, -2
Tensile Modulus 0.703 GPa102 ksiISO 527-1, -2
Flexural Modulus 0.660 GPa95.7 ksiISO 178
Izod Impact, Notched (ISO) 94.6 kJ/m²
@Temperature 23.0 °C
45.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 24.0 J
@Temperature -30.0 °C
17.7 ft-lb
@Temperature -22.0 °F
Instrumented Peak Energy; ASTM D3763

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 1120 H Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
Pinnacle Polymers 1120 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat

PMO824 / 53813

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.