MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds TASK® 18 (C-1508) Rigid Urethane Casting Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 18 is a relatively low viscosity aluminum filled urethane casting resin that was developed specifically for making short run vacuum forming molds. When Parts A and B are mixed in proper proportion, TASK™ 18 cures overnight at room temperature with negligible shrinkage to a very hard plastic that has a very high compressive and flexural strength. Cured TASK™ 18 can be polished, machined, drilled, painted, etc. TASK™ 18 is also used to make industrial production parts, prototype parts and tracing patterns.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccASTM D-1475
Viscosity 4400 cP4400 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.00060 cm/cm0.00060 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D-2240
Tensile Strength, Ultimate 22.4 MPa3250 psiASTM D-638
Elongation at Break 1.0 %1.0 %ASTM D-638
Tensile Modulus 3.54 GPa514 ksiASTM D-638
Flexural Strength 73.8 MPa10700 psiASTM D-790
Flexural Modulus 0.593 GPa86.0 ksiASTM D-790
Compressive Strength 58.1 MPa8420 psiASTM D-695
Compressive Modulus 0.671 GPa97.3 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 65.0 °C149 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hourHandling Time
Pot Life 20.0 min20.0 minASTM D-2471
 
Descriptive Properties
ColorMetal Gray
Mix Ratio26A:100Bby weight
Specific Volume17.6[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN043 / 296744

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.