MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds TASK® 18 (C-1508) Rigid Urethane Casting Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 18 is a relatively low viscosity aluminum filled urethane casting resin that was developed specifically for making short run vacuum forming molds. When Parts A and B are mixed in proper proportion, TASK™ 18 cures overnight at room temperature with negligible shrinkage to a very hard plastic that has a very high compressive and flexural strength. Cured TASK™ 18 can be polished, machined, drilled, painted, etc. TASK™ 18 is also used to make industrial production parts, prototype parts and tracing patterns.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/ccASTM D-1475
Viscosity 4400 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.00060 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88ASTM D-2240
Tensile Strength, Ultimate 3250 psiASTM D-638
Elongation at Break 1.0 %ASTM D-638
Tensile Modulus 514000 psiASTM D-638
Flexural Strength 10700 psiASTM D-790
Flexural Modulus 86000 psiASTM D-790
Compressive Strength 8420 psiASTM D-695
Compressive Modulus 97300 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 65.0 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hourHandling Time
Pot Life 20.0 minASTM D-2471
 
Descriptive Properties
ColorMetal Gray
Mix Ratio26A:100Bby weight
Specific Volume17.6[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN043 / 296744

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.