MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Tecophilic® HP-60D-20 Hydrophilic TPU – Extrusion Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Medical Grade Aliphatic Hydrophilic Polyether-based Thermoplastic Polyurethanes (TPUs)

Features: Specially formulated to absorb a large equilibrium water content.

Process: Extrusion primarily but can also be Injection Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Water Absorption 20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43ASTM D2240
Tensile Strength, Ultimate 5100 psiWet; ASTM D412
 8900 psiDry; ASTM D412
Elongation at Break 390 %Wet; ASTM D412
 430 %Dry; ASTM D412
Flexural Modulus 4300 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 221 °CInjection
Front Barrel Temperature 227 °CInjection
Nozzle Temperature 227 °CInjection
Zone 1 176.6 °CExtrusion
Zone 2 182.8 °CExtrusion
Zone 3 187.7 °CExtrusion
Zone 4 193.3 °CExtrusion
Adapter Temperature 187.7 °CExtrusion
Die Temperature 187.7 °CExtrusion
Melt Temperature >= 246 °CInjection
Mold Temperature 32.0 - 54.0 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecophilic® HP-60D-35 Hydrophilic TPU – Extrusion Grade
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Lubrizol LifeSciences Tecophilic® HP-93A-100 Hydrophilic TPU – Extrusion Grade

PLUBR9078 / 203645

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.