MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for low head pipe seal applications and complies with EN 681-2:2000. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

  • Recommended for applications requiring excellent flex fatigue resistance
  • Recommended for applications requiring excellent ozone resistance
  • Good resistance to compression set.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56.12 in; ASTM D2240
 56Air at 158°F, 96 hr; ASTM D573
Tensile Strength at Break 720 psiAir at 158°F, 96 hr; ASTM D573
 750 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 290 psiAcross Flow; ASTM D412
Elongation at Break 368.6 %Air at 158°F, 96 hr; ASTM D573
 380 %Across Flow; ASTM D412
Tear Strength 51.0 pli212°F, Die C; ASTM D624
 165 pli73°C, Die C; ASTM D624
Compression Set 25 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -78.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr1.16
ColorBlack
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934E Thermoplastic Elastomer
Avient OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer

PADVA040 / 22730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.