MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15X-2 One Component, Non-Yellowing UV Curable Adhesive
Categories: Polymer; Thermoset

Material Notes: Key Features:
  • Low viscosity
  • Superior non-yellowing properties
  • Excellent physical properties
  • Low shrinkage upon cure
Product Description: Master Bond UV15X-2 is a high performance UV curable system for bonding, coating, sealing and encapsulation. It serves up a brisk combination of superior physical strength properties, very low shrinkage upon curing along with superior non-yellowing properties. UV15X-2 bonds well to a wide variety of substrates including glass, metals, ceramics and many plastics, especially polycarbonates and acrylics. It is particularly useful for bonding dissimilar substrates, and for withstanding rigorous thermal cycling. It has outstanding chemical resistance to water, oils, fuels, acids and bases. Other favorable characteristics include top notch electrical insulation values, fine dimensional stability and superior abrasion resistance. The service temperature range is -80°F to 300°F. Master Bond UV15X-2 system is not oxygen inhibited and cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections up to 1/4 inch. However, when bonding, sections of a few thousandths of an inch are more than adequate. No solvents or vapors are released during the curing process. UV15X-2 is used in fiber-optic, optical, electronic, microelectronic, semiconductor and laser applications, among many others.

Product Advantages:

  • One component system; no mixing needed
  • Cures very fast upon UV light exposure
  • No oxygen inhibition while curing; no special inert atmosphere required
  • Combines impressive physical strength and electrical insulation properties
  • Excellent light transmission, superb optical clarity
  • Noteworthy dimensional stability and abrasion resistance

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/cc
Viscosity 3000 - 9000 cP3000 - 9000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 70>= 70
Tensile Strength 41.4 - 48.3 MPa6000 - 7000 psi
Tensile Modulus 2.07 - 2.41 GPa300 - 350 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.6
@Frequency 60 Hz
3.6
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg 80.0 - 85.0 °C176 - 185 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond UV15X-6NM-2 One Component UV Curing Urethane Acrylate
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications
Master Bond UV15X-5 One Component High Viscosity UV Curable System
Master Bond UV15X-2GT One Component, UV Curable Glob Top Compound
Master Bond UV15TK High Temperature Resistant One Component UV Curable System

PMASTM976 / 185569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.