MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Iupilon® ECF 2010R Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: 10% carbon fiber. Carbon fiber reinforced (flame retardant) grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics. Superior impact strength. Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC. Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Water Absorption 0.11 %
@Temperature 23.0 °C
Immersion
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
@Thickness 3.20 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 113 MPaISO 527-1,2
Elongation at Break 4.0 %ISO 527-1,2
Tensile Modulus 8000 MPaISO 527-1,2
Flexural Strength 160 MPaISO 178
Flexural Modulus 7200 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²ISO 179-1,2
Charpy Impact, Notched 8.00 kJ/m²ISO 179-1,2
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 146 °CISO 75-1,2
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-2
@Thickness 0.800 mm
 V-0
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® B-4120R Carbon Fiber Reinforced Polycarbonate
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced
Solvay APC-2/AS4 PEEK Plus Carbon Fiber Reinforced Unidirectional Tape
RTP Company RTP 381 EM Polycarbonate (PC), Carbon Fiber - Easy Molding - Self Extinguishing - Halogen Free - UL94 V-2
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release

PMITSU9276 / 191949

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.