MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teijin Panlite® B-4120R Carbon Fiber Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: Carbon Fiber Reinforced grades-20% carbon fiber, high flame resistant grade, non-bromine / non-phosphor type. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Filter / reinforcement: Carbon fiber,20% filler by weight. Features: Creep resistant, high Rigidity, bromine free. Uses: industrial applications. Appearance: black. Forms: pellets. Processing Method: Injection Molding.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 0.140 %
@Temperature 23.0 °C,
Time 86400 sec
0.140 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.00020 - 0.0020 cm/cm
@Thickness 4.00 mm
0.00020 - 0.0020 in/in
@Thickness 0.157 in
Teijin method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 4.00 mm
0.0030 - 0.0050 in/in
@Thickness 0.157 in
Teijin method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psiISO 527-2/5
Elongation at Break 1.5 %1.5 %ISO 527-2/5
Tensile Modulus 13.6 GPa1970 ksiISO 527-2/1
Flexural Strength 185 MPa26800 psi2.0 mm/min; ISO 178
Flexural Modulus 12.0 GPa1740 ksi2.0 mm/min; ISO 178
Charpy Impact Unnotched 2.80 J/cm²13.3 ft-lb/in²ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 - 1000 ohm-cm10 - 1000 ohm-cmIEC 60093
Surface Resistance 1.0 - 100 ohm1.0 - 100 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °Funannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 147 °C297 °Funannealed; ISO 75-2/A
Vicat Softening Point 152 °C306 °FISO 306/B50
UL RTI, Electrical 80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
UL RTI, Mechanical without Impact 80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
Flammability, UL94 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teijin Panlite® EN-8615N EMS Shield Grade Polycarbonate
EMS-Grivory Grilamid® L 25 W 40 ESD PA12
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Teijin Panlite® B-4110R Carbon Fiber Reinforced Polycarbonate
Teijin Panlite® B-4130R Carbon Fiber Reinforced Polycarbonate

PTEIH976 / 191647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.