MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zoltek™ PX30 PW03 (Plain Weave) Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 Woven Carbon Fabrics tailorability results from controlling the yield on rovings and yarns, and allows for a variety of finished composite thicknesses. The spun yarns have many surface fibrils that protrude in various directions at various lengths from the surface. This fiber loft contributes to high cross-ply tensile and interlaminar shear strengths for 2-D composite materials. Contour conformation without wrinkling is another advantage of spun yarn fabrics. ZOLTEK PX30 materials undergo high temperature carbonization process, involving a long temperature soak time, resulting in a very thermally stable and chemically pure fabric with low oxidation rate.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
Thickness 406 microns16.0 milCured
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00140 ohm-cm0.00140 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %
 
Descriptive Properties
Areal Weight115 g/m2
ColorBlack
Oxidation Rate1% per hour @ 932°F
Roll Length73 m
Roll Width838 mm
Warp and Fill175 x 175 yarns/10cm
Yarn Input2/27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ OX SW08 (Satin Weave) Oxidized PAN Fiber Fabric
E-Glass Fiber, Generic
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Fibre Glast 660 6K, 5HS Weave Carbon Fiber Fabric
Solvay CYCOM® 934 Epoxy - Pitch High Modulus Carbon Fiber Reinforced Unidirectional Tape Laminate

ECZO833 / 232308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.