MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zoltek™ OX SW08 (Satin Weave) Oxidized PAN Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK OX satin weaves and circular knits are produced from 100% ZOLTEK OX yarn. These fabrics are characterized by high LOI%, excellent stretch, no melt-no drip and a soft hand for apparel applications. Recommended use: Protective apparel, furniture & bedding.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³fiber
Thickness 1200 microns47.2 milCured
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.00e+8 ohm-cm8.00e+8 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Oxygen Index >= 40 %>= 40 %Fiber property.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 62 %62 %
Hydrogen, H 4.5 %4.5 %
Nitrogen, N 21.5 %21.5 %
O2 12 %12 %
Sodium, Na <= 0.10 %<= 0.10 %
Trace Metals <= 0.010 %<= 0.010 %
 
Descriptive Properties
Areal Weight471 g/m2
ColorBlack
Construction8 harness satin
Fiber Diameter (µm)12.5
Organic SolventsExcellent resistance
Roll Length45m. Satin Weave SW08
Roll Width129 cm. Satin Weave SW08
Strong AcidsGood resistance
Strong BasesPoor resistance
Weak AcidsExcellent resistance
Weak BasesGood resistance
Yarn Input2/10 worsted count

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX30 PW03 (Plain Weave) Carbon Fiber Fabric
Fibre Glast 660 6K, 5HS Weave Carbon Fiber Fabric
Solvay CYCOM® 934 Epoxy - Pitch High Modulus Carbon Fiber Reinforced Unidirectional Tape Laminate
Graphite, Carbon, C
Abatron AboCast 10-5/AboCure 3-4 Epoxy

ECZO827 / 232298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.