MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics K-Shield® BF Paper Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: RFC Fiber Class. K-Shield BF Paper is an organic-free paper produced from premium, cleaned Kaowool high-purity fibers in a unique paper-making process. The cleaning process of these special fibers dramatically improves the thermal conductivity and insulating value of the product. K-Shield BF paper offers excellent thermal resistance and good handling strength with no off-gassing.

Applications:

  • Separating media to prevent sticking
  • Vacuum heat treating furnaces
  • Parting agent in brazing and heat treating
  • Powered Metal sintering
  • Applications that require good fired strengths
  • Commercial Appliance Insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.128 - 0.160 g/cc
Loss On Ignition <= 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.00 - 1.70 MPa
 1.00 - 1.70 MPafired
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0500 W/m-K
@Temperature 260 °C
 0.0900 W/m-K
@Temperature 538 °C
 0.120 W/m-K
@Temperature 816 °C
 0.170 W/m-K
@Temperature 1093 °C
Maximum Service Temperature, Air <= 1260 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
Al2O3 51 %
SiO2 49 %
 
Descriptive Properties
Classification Temperature (°C)1316
Colorwhite
Fiber Index (%)75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool ™ Cement & Veneering Cement
Morgan Advanced Ceramics Kaowool® Paper 333-E Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Papers AZS Paper Ceramic Fiber

CMORF6499 / 203283

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.