MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Acrylic, General Purpose, Molded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.700 - 1.30 g/cc0.0253 - 0.0470 lb/in³Average value: 1.17 g/cc Grade Count:279
Water Absorption 0.300 - 2.00 %0.300 - 2.00 %Average value: 0.423 % Grade Count:125
Moisture Absorption at Equilibrium 0.300 - 0.600 %0.300 - 0.600 %Average value: 0.399 % Grade Count:29
Water Absorption at Saturation 0.300 - 2.20 %0.300 - 2.20 %Average value: 1.23 % Grade Count:21
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cm0.00200 - 0.00800 in/inAverage value: 0.00446 cm/cm Grade Count:214
Melt Flow 0.112 - 40.0 g/10 min0.112 - 40.0 g/10 minAverage value: 7.93 g/10 min Grade Count:279
Spiral Flow 22.0 - 51.0 cm8.66 - 20.1 inAverage value: 32.1 cm Grade Count:22
 130 - 370 cm
@Temperature 230 - 250 °C
51.2 - 146 in
@Temperature 446 - 482 °F
Average value: 229 cm Grade Count:4
 130 - 370 cm
@Thickness 2.00 - 2.00 mm
51.2 - 146 in
@Thickness 0.0787 - 0.0787 in
Average value: 229 cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 40.0 - 54.040.0 - 54.0Average value: 46.0 Grade Count:3
Hardness, Rockwell M 18.0 - 10118.0 - 101Average value: 84.4 Grade Count:130
Hardness, Rockwell R 69.069.0Average value: 69.0 Grade Count:4
Ball Indentation Hardness 170 - 190 MPa24700 - 27600 psiAverage value: 179 MPa Grade Count:21
Tensile Strength, Ultimate 19.3 - 85.0 MPa2800 - 12300 psiAverage value: 64.6 MPa Grade Count:239
Tensile Strength, Yield 25.0 - 85.0 MPa3630 - 12300 psiAverage value: 60.5 MPa Grade Count:52
Elongation at Break 1.00 - 85.0 %1.00 - 85.0 %Average value: 10.1 % Grade Count:284
Elongation at Yield 2.00 - 6.00 %2.00 - 6.00 %Average value: 4.54 % Grade Count:58
Modulus of Elasticity 0.950 - 3.79 GPa138 - 550 ksiAverage value: 2.93 GPa Grade Count:234
Flexural Yield Strength 33.1 - 143 MPa4800 - 20700 psiAverage value: 103 MPa Grade Count:238
Flexural Modulus 1.17 - 3.59 GPa170 - 520 ksiAverage value: 2.88 GPa Grade Count:131
Compressive Yield Strength 36.5 - 117 MPa5300 - 17000 psiAverage value: 99.7 MPa Grade Count:9
Izod Impact, Notched 0.107 - 1.47 J/cm0.200 - 2.76 ft-lb/inAverage value: 0.303 J/cm Grade Count:178
 0.240255 - 0.37373 J/cm
@Temperature 0.000 - 0.000 °C
0.450096 - 0.70015 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:6
 0.10678 - 0.80085 J/cm
@Temperature 0.000 - 0.000 °C
0.20004 - 1.5003 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:10
 0.10678 - 0.80085 J/cm
@Thickness 3.17 - 6.35 mm
0.20004 - 1.5003 ft-lb/in
@Thickness 0.125 - 0.250 in
Average value: 0.463 J/cm Grade Count:10
 0.26695 - 0.85424 J/cm
@Diameter 6.35 - 6.35 mm
0.50011 - 1.6003 ft-lb/in
@Diameter 0.250 - 0.250 in
Average value: 0.463 J/cm Grade Count:6
 0.26695 - 0.85424 J/cm
@Temperature 0.000 - 0.000 °C
0.50011 - 1.6003 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:6
Izod Impact, Notched (ISO) 1.30 - 19.0 kJ/m²0.619 - 9.04 ft-lb/in²Average value: 3.13 kJ/m² Grade Count:23
Izod Impact, Unnotched (ISO) 2.10 kJ/m²0.999 ft-lb/in²Average value: 2.10 kJ/m² Grade Count:4
Charpy Impact Unnotched 1.00 J/cm² - NB4.76 ft-lb/in² - NBAverage value: 2.59 J/cm² Grade Count:90
Charpy Impact, Notched 0.120 - 1.30 J/cm²0.571 - 6.19 ft-lb/in²Average value: 0.198 J/cm² Grade Count:65
Gardner Impact 0.226 - 6.33 J0.167 - 4.67 ft-lbAverage value: 0.430 J Grade Count:104
Falling Dart Impact 2.17 - 18.6 J1.60 - 13.7 ft-lbAverage value: 10.7 J Grade Count:4
Tensile Creep Modulus, 1 hour 1800 - 2700 MPa261000 - 392000 psiAverage value: 2460 MPa Grade Count:9
Tensile Creep Modulus, 1000 hours 1200 - 1800 MPa174000 - 261000 psiAverage value: 1580 MPa Grade Count:10
Taber Abrasion, mg/1000 Cycles 16.516.5Average value: 16.5 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 - 1.00e+17 ohm-cm1.00e+10 - 1.00e+17 ohm-cmAverage value: 3.26e+15 ohm-cm Grade Count:38
Surface Resistance 2.60e+9 - 1.00e+16 ohm2.60e+9 - 1.00e+16 ohmAverage value: 1.78e+15 ohm Grade Count:27
Dielectric Constant 2.44 - 4.002.44 - 4.00Average value: 3.44 Grade Count:35
Dielectric Strength 15.0 - 60.0 kV/mm380 - 1520 kV/inAverage value: 27.2 kV/mm Grade Count:42
Dissipation Factor 0.0200 - 0.1900.0200 - 0.190Average value: 0.0497 Grade Count:37
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:16
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 150 µm/m-°C16.7 - 83.3 µin/in-°FAverage value: 70.7 µm/m-°C Grade Count:180
 72.0 - 149.4 µm/m-°C
@Temperature -17.8 - 156 °C
40.0 - 83.00 µin/in-°F
@Temperature 0.000 - 312 °F
Average value: 94.9 µm/m-°C Grade Count:26
Specific Heat Capacity 1.46 - 1.50 J/g-°C0.349 - 0.359 BTU/lb-°FAverage value: 1.49 J/g-°C Grade Count:10
Thermal Conductivity 0.187 - 0.216 W/m-K1.30 - 1.50 BTU-in/hr-ft²-°FAverage value: 0.199 W/m-K Grade Count:17
Maximum Service Temperature, Air 50.0 - 100 °C122 - 212 °FAverage value: 86.8 °C Grade Count:89
Deflection Temperature at 0.46 MPa (66 psi) 73.0 - 109 °C163 - 228 °FAverage value: 97.2 °C Grade Count:65
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 106 °C125 - 223 °FAverage value: 89.3 °C Grade Count:230
Vicat Softening Point 58.3 - 119 °C137 - 246 °FAverage value: 101 °C Grade Count:273
Heat Distortion Temperature 85.0 - 105 °C185 - 221 °FAverage value: 96.4 °C Grade Count:7
Glass Transition Temp, Tg 102 - 122 °C216 - 252 °FAverage value: 110 °C Grade Count:22
Flammability, UL94 HBHBGrade Count:166
Oxygen Index 18.0 %18.0 %Average value: 18.0 % Grade Count:7
Glow Wire Test 650 - 700 °C1200 - 1290 °FAverage value: 662 °C Grade Count:30
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49 - 1.521.49 - 1.52Average value: 1.49 Grade Count:127
Haze 0.300 - 100 %0.300 - 100 %Average value: 8.77 % Grade Count:171
Yellow Index -7.50 - 6.50 %-7.50 - 6.50 %Average value: 0.758 % Grade Count:25
Transmission, Visible 40.0 - 93.0 %40.0 - 93.0 %Average value: 90.3 % Grade Count:240
UV Transmittance 0.190 - 92.0 %0.190 - 92.0 %Average value: 77.4 % Grade Count:23
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 265 °C350 - 509 °FAverage value: 237 °C Grade Count:35
Nozzle Temperature 193 - 260 °C380 - 500 °FAverage value: 228 °C Grade Count:8
Adapter Temperature 230 - 240 °C446 - 464 °FAverage value: 235 °C Grade Count:4
Die Temperature 220 - 260 °C428 - 500 °FAverage value: 240 °C Grade Count:14
Melt Temperature 150 - 260 °C302 - 500 °FAverage value: 227 °C Grade Count:56
Mold Temperature 30.0 - 107 °C86.0 - 225 °FAverage value: 63.3 °C Grade Count:54
Roll Temperature 80.0 - 100 °C176 - 212 °FAverage value: 90.0 °C Grade Count:4
Drying Temperature 60.0 - 109 °C140 - 228 °FAverage value: 83.7 °C Grade Count:63
Injection Pressure 58.8 - 147 MPa8530 - 21300 psiAverage value: 104 MPa Grade Count:15
Annealing Temperature 60.0 - 90.0 °C140 - 194 °FAverage value: 77.1 °C Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polycarbonate, Molded
Overview of materials for Acrylic, Impact Modified, Molded
Overview of materials for Acrylic, Cast

O1300 / 77859

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.