MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Röchling Polystone® P EL Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product characteristics:
  • Electrically conductive
Product applications:
  • Ventilation technology
  • Electrical industry
  • Pump engineering

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiDIN EN ISO 527
Elongation at Break >= 74 %>= 74 %DIN EN ISO 527
Modulus of Elasticity 1.40 GPa203 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmDIN EN 62631-3-1
Surface Resistance 1000 ohm1000 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 11357-3
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Borealis BD212CF Polypropylene Copolymer
Borealis BC612WG Polypropylene Copolymer
Borealis BB213CF Polypropylene Copolymer
Borealis BA11CF Polypropylene Copolymer

PROCH9251 / 232954

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.