MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.

Polypropylene PPC 8780 has been specially developed for the injection molding of lids combining flexibility and low warpage.

Polypropylene PPC 8780 is also suitable for extrusion coating.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccISO 1183
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
18 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080ISO 2039-2
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-2
Elongation at Yield 5.5 %5.5 %ISO 527-2
Tensile Modulus 1.05 GPa152 ksiISO 527-2
Flexural Modulus 0.950 GPa138 ksiISO 178
Izod Impact, Notched (ISO)  5.50 kJ/m²
@Temperature -20.0 °C
2.62 ft-lb/in²
@Temperature -4.00 °F
ISO 180
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched  1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 1.60 J/cm²
@Temperature -20.0 °C
7.61 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °F120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °F120°C per hour; ISO 752
Vicat Softening Point  65.0 °C
@Load 5.10 kg
149 °F
@Load 11.2 lb
50°C per hour; ISO 306
 135 °C
@Load 1.02 kg
275 °F
@Load 2.25 lb
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
BASF Novolen® 1102 K Polypropylene
Addiplast Addilene H 242 M40 Polypropylene Homopolymer
Borealis BL2571 High Density Polyethylene
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications

PTOTAL853 / 130578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.