MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Park Aerospace Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and processing windows.

Applications/Qualifications:

  • Fine-Line Multilayers
  • Surface-Mount Multilayers
  • MCM-Ls
  • PCMCIA Cards
  • Wireless Communications
  • Bluetooth Modules
  • Automotive
  • RoHS Compliant
  • Meets IPC-4101/21 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.92 g/cc0.0694 lb/in³50% Resin Content; Internal Method
Water Absorption 0.10 %0.10 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 24.1 GPa3500 ksiY; ASTM D3039
 28.3 GPa4100 ksiX; ASTM D3039
Poissons Ratio 0.140.14Y; ASTM D3039
 0.160.16X; ASTM D3039
Peel Strength 1.23 kN/m7.00 pliat elevated temperature; IPC-TM-650.2.4.8.2a
 1.58 kN/m9.00 pliafter exposure to process solutions; IPC-TM-650.2.4.8
 1.58 kN/m9.00 pliafter solder float; IPC-TM-650.2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmE - 24/125; IPC-TM-650.2.5.17.1
 1.00e+14 ohm-cm1.00e+14 ohm-cmC - 96/35/90; IPC-TM-650.2.5.17.1
Surface Resistance 1.00e+12 ohm1.00e+12 ohmE - 24/125; IPC-TM-650.2.5.17.1
 1.00e+13 ohm1.00e+13 ohmC - 96/35/90; IPC-TM-650.2.5.17.1
Dielectric Constant  4.1
@Frequency 1e+9 Hz
4.1
@Frequency 1e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
 4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Dielectric Strength 49.2 kV/mm1250 kV/inIPC-TM-650.2.5.6.2
Dielectric Breakdown >= 50000 V>= 50000 VIPC-TM-650.2.5.6
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Arc Resistance 65 sec65 secIPC-TM-650.2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 - 16.0 µm/m-°C
@Temperature -40.0 - 125 °C
6.67 - 8.90 µin/in-°F
@Temperature -40.0 - 257 °F
X/Y; IPC-TM-650.2.4.41
Specific Heat Capacity 1.21 - 1.38 J/g-°C0.290 - 0.330 BTU/lb-°FASTM E1461-92
Thermal Conductivity 0.300 - 0.401 W/m-K2.08 - 2.78 BTU-in/hr-ft²-°FASTM E1461-92
Glass Transition Temp, Tg 130 °C266 °FTMA; IPC-TM-650.2.4.24c
 140 °C284 °FDSC; IPC-TM-650.2.4.25c
Decomposition Temperature 300 °C572 °F5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.7IPC-TM-650.2.3.4.3
Pressure CookerPass60 min then solder dip @288ºC until failure (max 10 min.); IPC-TM-650.2.6.16 (modified)
T260 (minutes)8-12IPC-TM-650.2.4.24.1
Z Axis Expansion (%)4.550ºC to 260ºC; IPC-TM-650.2.4.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
Park Aerospace Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Park Aerospace Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg
Park Aerospace Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg

PPARK110 / 89382

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.