MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® iC 4800 3DF PEEK, Mineral Fiber Reinforced
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: VESTAKEEP® iC4800 3DF is an opaque, natural colored, high viscosity polyether ether ketone (PEEK) filament based on VESTAKEEP® iC4800 G resin. It contains calcium phosphates to enhance osseointegration. It therefore belongs to the VESTAKEEP® Fusion product family.
Dry properties listed below
Industrial Sector: Medical Device, 3D Printings Processing: 3D Printing
Delivery form: (Mono)filament
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering
Electrical: Insulating
Conformity: Biocompatibility, Medical application
Additives: Mineral fillers
Applications: Medical implants
Processing: Fused deposition molding, Additive manufacturing
Special Characteristics: Phosphorus-free, PTFE-free, High impact strength, Semi-crystalline, High viscosity, Self-extinguishing
Features: Low odor, Non-corrosive
Regulatory: US Pharmacopeia Class VI conformity
Color: Grey
Additives: Inorganic fillers
Chemical Resistance: Acid resistance, Solvent resistance, Oxidation resistance, Radiation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Water Absorption 0.400 %Sim to ISO 62
Melt Flow 10.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 90.0 MPaISO 527
Tensile Strength, Yield 90.0 MPaISO 527
Elongation at Break 10.0 %ISO 527
Elongation at Yield 4.00 %ISO 527
Tensile Modulus 4350 MPaISO 527
Charpy Impact, Notched 4.70 kJ/m²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °CISO 11357-1/-3
Glass Transition Temp, Tg 145 °C2nd heating, onset; ISO 11357
 155 °C2nd heating, midpoint; ISO 11357
 
Processing PropertiesOriginal ValueComments
Recrystallization Temperature 285 °C20 K/min; ISO 11357
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7873 / 325005

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.