VESTAKEEP® iC4800 3DF is an opaque, natural colored, high viscosity polyether ether ketone (PEEK) filament based on VESTAKEEP® iC4800 G resin. It contains calcium phosphates to enhance osseointegration. It therefore belongs to the VESTAKEEP® Fusion product family. Dry properties listed below Industrial Sector: Medical Device, 3D Printings Processing: 3D Printing Delivery form: (Mono)filament Optics: Opaque Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering Electrical: Insulating Conformity: Biocompatibility, Medical application Additives: Mineral fillers Applications: Medical implants Processing: Fused deposition molding, Additive manufacturing Special Characteristics: Phosphorus-free, PTFE-free, High impact strength, Semi-crystalline, High viscosity, Self-extinguishing Features: Low odor, Non-corrosive Regulatory: US Pharmacopeia Class VI conformity Color: Grey Additives: Inorganic fillers Chemical Resistance: Acid resistance, Solvent resistance, Oxidation resistance, Radiation resistance, General chemical resistanceInformation provided by Evonik. |