MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applications where low closure force and dust sealing are critical. Available in various thicknesses and manufactured in roll form.

Features and Benefits:

  • Ultra low softness allows designers to use less force to seal enclosures and still protect their device from the environment.
  • High compressibility allows material to conform to variable width gaps, thereby allowing more design flexibility.
  • Excellent memory and low stress relaxation reduces maintenance costs associated with gasket failures due to compression set and softening.
  • Resistance to ultraviolet light, ozone, extreme temperatures and flame enables consistent performance in all environments.
  • Color: black
  • Thickness: 0.125 in to 0.500 in
  • Standard Width: 0.500 in to 36.0 in

Applications:

  • Vibration isolation in electronic components and transportation vehicles
  • Low closure force gaskets within portable electronics such as laptops and LCD screens within aircraft and rail interiors
  • Fire retardant thermal insulation

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.0 lb/ft³ASTM D1056
Thickness 125 - 500 milRange of Thicknesses Available
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.0 psiASTM D412
Elongation at Break 80 %ASTM D412
Compressive Yield Strength 1.50 psi
@Strain 25 %
ASTM D1056
Compression Set 1.0 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D1056
 5.0 %
@Temperature 100 °C,
Time 79200 sec
ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0also HF-1
Flame Spread Index <= 25Is; ASTM E162
Smoke Density 1.5 min<20; Ds; ASTM E662
 4.0 min<50; Ds; ASTM E662
 
Descriptive Properties
Toxic Gas EmissionsPassSMP-800C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam
General Plastics LAST-A-FOAM® FP-5018 Polyurethane Foam
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge

PROGA904 / 138344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.