MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Pyro-Packing R
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyro-Packing is used to fill gaps or small spaces in ceramic fiber module linings where standard shapes are not practical or cost effective. Manufactured by cutting pieces of monolithic Pyro-Log, Pyro-Packing is available in R Grade, ZR Grade and now in C Grade. Densities range from 8 pcf to 15 pcf (128 to 240 kg/m3) which better match the surrounding Pyro-Bloc lining and offers higher densities when compared to traditional ceramic fiber blanket packing. A typical application would be to fill gaps or small spaces where standard shapes are not practical.

Features:

  • Manufactured from Pyro-Log Fiber
  • Used to fill small gaps impractical for standard module shapes
  • Available in compressed densities from 8 to 15 pcf (128 to 240 kg/m3)
  • Matches packing with density of surrounding Pyro-Bloc module lining
  • Applications:

  • Low mass kiln cars
  • Fired heater floors
  • Back up insulation for insulating firebrick and castable lining
  • Fill gaps or small spaces where standard shapes are not practical
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.128 g/cc0.00462 lb/in³Available in multiple densities
     0.160 g/cc0.00578 lb/in³Available in multiple densities
     0.192 g/cc0.00694 lb/in³Available in multiple densities
     0.240 g/cc0.00867 lb/in³Available in multiple densities
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0706 W/m-K
    @Temperature 260 °C
    0.490 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    15 pcf; ASTM C201
     0.0720 W/m-K
    @Temperature 260 °C
    0.500 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    12 pcf; ASTM C201
     0.0749 W/m-K
    @Temperature 260 °C
    0.520 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    10 pcf; ASTM C201
     0.0764 W/m-K
    @Temperature 260 °C
    0.530 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    8 pcf; ASTM C201
     0.121 W/m-K
    @Temperature 538 °C
    0.840 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    15 pcf; ASTM C201
     0.138 W/m-K
    @Temperature 538 °C
    0.960 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    12 pcf; ASTM C201
     0.150 W/m-K
    @Temperature 538 °C
    1.04 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    10 pcf; ASTM C201
     0.163 W/m-K
    @Temperature 538 °C
    1.13 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    8 pcf; ASTM C201
     0.206 W/m-K
    @Temperature 816 °C
    1.43 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    15 pcf; ASTM C201
     0.239 W/m-K
    @Temperature 816 °C
    1.66 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    12 pcf; ASTM C201
     0.261 W/m-K
    @Temperature 816 °C
    1.81 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    10 pcf; ASTM C201
     0.284 W/m-K
    @Temperature 816 °C
    1.97 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    8 pcf; ASTM C201
     0.316 W/m-K
    @Temperature 1090 °C
    2.19 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    15 pcf; ASTM C201
     0.353 W/m-K
    @Temperature 1090 °C
    2.45 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    12 pcf; ASTM C201
     0.388 W/m-K
    @Temperature 1090 °C
    2.69 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    10 pcf; ASTM C201
     0.425 W/m-K
    @Temperature 1090 °C
    2.95 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    8 pcf; ASTM C201
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1200 °C2200 °FContinuous
     1320 °C2400 °FRating
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 47 %47 %
    SiO2 53 %53 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Anderman Ceramics EZY 88 Zirconia, 88%, Fully Yttria-Stabilized
    Sharadaa Ceramics Calcium Silicate Block
    Sharadaa Ceramics REFCAST C High Alumina Castables
    Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables
    Thermal Ceramics K-Shield Felt AG/Min-K Composite

    CTHERM081 / 2401

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.