MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Anderman Ceramics EZY 88 Zirconia, 88%, Fully Yttria-Stabilized
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.

Key Words: ZrO2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.85 g/cc0.211 lb/in³
Open Porosity 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 8.08.0
Flexural Strength 207 MPa30000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  10000 ohm-cm
@Temperature 600 °C
10000 ohm-cm
@Temperature 1110 °F
 1.00e+13 ohm-cm
@Temperature 20.0 °C
1.00e+13 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.5 µm/m-°C5.83 µin/in-°F
Thermal Conductivity 2.50 W/m-K
@Temperature 20.0 - 100 °C
17.4 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1800 °C3270 °F
 
Component Elements PropertiesMetricEnglishComments
Y2O3 12 %12 %
ZrO2 88 %88 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EM80P Corundum
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized
Advanced Ceramics ALC 1082 (C-786) Alumina
Advanced Ceramics ALC 1081 (C-786) Alumina
Anderman Ceramics EA95 Sintered Alumina, 95%

CANDER14 / 104649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.