MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Vac-Pak® UHT750 Vacuum bagging film
Categories: Polymer; Film

Material Notes: Description: Vacuum bagging film. Ideally suited to aerospace applications.

Features & Benefits:

  • High performance clear amber polyimide film suitable for cure cycles up to 426°C (800°F)
  • Suitable for use with high temperature thermoplastic matrix materials
  • Can also be used in release applications when treated with release agent

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.0 microns1.97 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 165 MPa24000 psiASTM D882
Elongation at Break 45 %45 %ASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 426 °C799 °F
 
Descriptive Properties
ColorAmber
Yield13.9 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay EF2000 Organosilicate Polymer
Hexcel® HexForce™ 383 Aramid Fabric
Hexcel® HexForce™ 328 Aramid Fabric
Solvay Polyifilm Polyimide Vacuum Bagging Film
Resinlab® RC8020 Anaerobic Retaining Compound

PCYTED307 / 180609

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.