MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lanxess Addovate® 390 PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: As a stabilizer for the production of polyurethane rigid foams.

Addovate 390 is a non-hydrolysable silicone stabilizer and may be used for the production of polyurethane rigid foams as e.g. insulations of appliances, pipe insulations, continuously or discontinuously produced panels as well as cavity foaming. Addovate 390 is a very versatile stabilizer of medium to high activity with additional excellent emulsifying properties. The use of Addovate 390 may be always recommended if either premixes or slow reacting formulations which contain incompatible raw materials (as e.g. polyols and physical blowing agents) should be stabilized. Due to the well balanced properties of Addovate 390 a reliable stabilization and a reduction of cell defects can be achieved in slow as well as fast systems. Addovate 390 is especially approved if pentane is used as physical blowing agent. In that case slow reacting systems with long flow distances (e.g. insulation of appliances) as well as fast reacting systems (e.g. continuous production of panels on double band laminators) can be produced reliably.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.07 g/cc0.0379 - 0.0387 lb/in³
pH 6.0 - 9.06.0 - 9.0
Viscosity 500 - 1000 cP500 - 1000 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 200 °C>= 392 °FInitial
Pour Point -23.3 °C-10.0 °F
Flash Point 117 °C243 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearanceyellow to slightly brown liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8223 / 208616

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.