MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool® Sealcoat HT Coating
Categories: Ceramic; Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: RCF. Kaowool Sealcoat HT is a pneumatically applied insulation material specifically designed for hot face lining applications up to 2600°F (1427°C). It’s unique composition of ceramic fibers, proprietary binders and special additives is designed to yield a density that provides optimal insulation characteristics for many applications.

Applications:

  • Grout refractory joints and gaps
  • Hot face coating over fiber or dense refractory
  • Seals furnace lining cracks
  • Back-up lining
  • Furnace maintenance and emergency repairs

Information provided by Morgan Advanced Materials

Key Words: Coating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 - 1.314 g/ccwet
 0.513 - 0.577 g/cc
@Temperature 110 °C
dried
Solids Content 41 %
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0900 W/m-K
@Temperature 260 °C
ASTM C201
 0.120 W/m-K
@Temperature 538 °C
ASTM C201
 0.160 W/m-K
@Temperature 816 °C
ASTM C201
 0.220 W/m-K
@Temperature 1093 °C
ASTM C201
Maximum Service Temperature, Air <= 1371 °CContinuous Use
Shrinkage 0.20 %
@Treatment Temp. 816 °C,
Time 86400 sec
 1.8 %
@Treatment Temp. 1093 °C,
Time 86400 sec
 2.9 %
@Treatment Temp. 1426 °C,
Time 86400 sec
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Al2O3 45 - 48 %after firing
Other 1.0 - 2.0 %
SiO2 51 - 54 %after firing
 
Descriptive Properties
Classification Temperature (°C)1427
Coloroff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Unikote® Coating S Coating
Morgan Advanced Ceramics Unikote® Coating M Coating
Morgan Advanced Ceramics Kaowool ™ White Cement Thermal Ceramic
Morgan Advanced Ceramics Kaowool Bulk Fiber Zirconia Fiber Thermal Ceramic
Morgan Advanced Ceramics Kaowool Bulk Fiber Standard Fibers

CMORF6154 / 202938

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.