MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.

Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and cosmetic containers.

Advantages: Excellent stress crack resistance, excellent resistance to most chemicals, outstanding rigidity with high impact strength, high melt strength and moderate die swell.

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.949 g/cc0.0343 lb/in³ASTM D1505
ESCR 100% Igepal® >= 1000 hour
@Thickness 1.90 mm,
Temperature 50.0 °C
>= 1000 hour
@Thickness 0.0748 in,
Temperature 122 °F
slit; ASTM D1693
Base Resin Melt Index 0.10 g/10 min0.10 g/10 minI2
 10 g/10 min10 g/10 minI21; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 36.3 MPa5260 psiASTM D638
Tensile Strength, Yield 30.4 MPa4410 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus 1.10 GPa160 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 °C356 °F
Front Barrel Temperature 190 °C374 °F
Head Temperature 190 °C374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Titanium, Ti
Alclad Aluminum 7075-T6, T651
Akro-Plastic Akromid® B3 1 L natural (4685) PA6 + PP, Dry, 30% Glass Filled
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer

PTITAN49 / 70415

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.