MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SAE J2477 AD 1400 Automotive Austempered Ductile Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Austempered Ductile Iron (ADI) is produced by heat-treating Ductile (Nodular) Iron using the austempering Process, (as exemplified in A.5), a specialized, isothermal heat treatment. When compared to conventional ductile iron, ADI can have over twice the strength for a given level of ductility. ADI can have fatigue strength comparable to that of cast and forged steels and that strength can be greatly enhanced by subsequent grinding, fillet rolling or shot peening. Although the first commercial application of ADI did not occur until 1972, the material has found applications in virtually every industrial market segment. Its principal attribute is its ability to replace steel forgings, castings and weldments at equal or lesser weight and at a reduced cost. It is also typically much less costly than aluminum and, with its high strength-to-weight ratio it has replaced cast aluminum parts at equal weight in some automotive applications.

The ausferrite matrix in ADI undergoes a strain transformation hardening when exposed to a high normal force. That effect makes machining of ADI challenging, but knowledge of this effect allows the machinist to adjust the feeds, speeds and tool angles to adequately compensate. This same strain transformation hardening is what gives ADI wear resistance better than its bulk hardness would indicate.

Other attributes of the material include, good noise dampening, fracture toughness and low temperature properties, and reasonable stiffness.

Applications
AD1400 is used where high strength and/or improved wear resistance are required.

Information provided by Applied Process Inc.

Key Words: ADI; SAE J2477
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 - 7.20 g/ccTypical value of ductile iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 388 - 477
@Diameter 2.80 - 3.10 mm
Tensile Strength at Break 1400 MPa
Tensile Strength, Yield 1100 MPa
Elongation at Break 2.0 %
Modulus of Elasticity 148 GPaASTM E111
Charpy Impact, Unnotched 35.0 JASTM E23
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.050 %
Antimony, Sb <= 0.0020 %
Arsenic, As <= 0.020 %
Bismuth, Bi <= 0.0020 %
Boron, B <= 0.00060 %
Cadmium, Cd <= 0.0050 %
Carbon, C 3.4 - 3.8 %
Chromium, Cr <= 0.10 %
Copper, Cu 0.75 - 0.85 %as needed
Iron, Fe 89.4 - 94 %balance
Lead, Pb <= 0.0020 %
Magnesium, Mg 0.020 - 0.0452 %
Manganese, Mn 0.25 - 0.35 %
Molybdenum, Mo 0.27 - 0.33 %as needed
Nickel, Ni 1.9 - 2.1 %as needed
Oxygen, O <= 0.0050 %
Phosphorus, P <= 0.040 %
Selenium, Se <= 0.030 %
Silicon, Si 2.3 - 2.7 %
Sulfur, S <= 0.020 %
Tellurium, Te <= 0.020 %
Tin, Sn <= 0.020 %
Titanium, Ti <= 0.040 %
Vanadium, V <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SAE J2477 AD 1600 Automotive Austempered Ductile Iron
ASTM A897 Grade 2 (150-100-07 or 150-110-7) Austempered Ductile Iron
ASTM A897/A897M-06 Grade 1 (130-90-09) Austempered Ductile Iron
SAE J2477 AD 1050 Automotive Austempered Ductile Iron
ASTM A897 Grade 3 (175-125-04) Austempered Ductile Iron

MDFEADI304 / 12075

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.