MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Duct 29121 Snap Cure Conductive Silver Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 29121 is 100% solids, two component silver filled epoxy designed for chip bonding in microelectronic and optoelectronic applications. TRA-DUCT 29121 is a soft, smooth paste. This two-part formulation is free of solvents. TRA-DUCT 29121 can be screen printed, machine dispensed or stamped.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.00 g/cc3.00 g/ccMixed, degassed
Viscosity 44500 cP
@Temperature 25.0 °C
44500 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 7.65 MPa1110 psiLap shear, alum to alum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 62.0 °C144 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  0.750 min
@Temperature 175 °C
0.0125 hour
@Temperature 347 °F
 5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
 15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
 90.0 min
@Temperature 80.0 °C
1.50 hour
@Temperature 176 °F
 720 min
@Temperature 50.0 °C
12.0 hour
@Temperature 122 °F
Pot Life 1440 min1440 min(1 day)
Working Life 2880 min2880 min
 
Descriptive Properties
Color Silver
Mix Ratio, parts by weight100/100Resin/Hardener
Thixotropic Index 3.21 rpm/10 rpm, cp #52

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Vyram™ 9271-75 Thermoplastic Rubber

PTRAC079 / 71007

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.