Higher wear resistance, service strength and impact toughness than YG6 and YG8. For drawing of steel<=¦µ50mm,non-ferrous metals and alloys into alloy bars and <=¦µ30mm tubes under high-stress conditions, and for fabricating of press dies with a largerdiameter and lower working load.Information provided by China Tungsten |