MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

China Tungsten YGR8 Tungsten Carbide with Rare Earth Additive
Categories: Ceramic; Carbide

Material Notes: Higher wear resistance, service strength and impact toughness than YG6 and YG8. For drawing of steel<=¦µ50mm,non-ferrous metals and alloys into alloy bars and <=¦µ30mm tubes under high-stress conditions, and for fabricating of press dies with a largerdiameter and lower working load.

Information provided by China Tungsten

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.6 - 14.9 g/cc0.527 - 0.538 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A >= 89.5>= 89.5
Flexural Strength >= 1650 MPa>= 239000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7039-T64
China Tungsten YT30 Tungsten Carbide for Cutting Tools
Bethlehem Steel BETHSTAR Grade 50 1/4 to 2-1/2 in. thick, killed steel plate
Crucible Steel CPM® 1V® High Alloy Tool Steel
China Tungsten YT712 Tungsten Carbide

NCHIN062 / 78904

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.