MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

3M Jet-melt™ 3748 V-O Light Yellow Adhesive: High-Melt Technology  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: The temperature control setting is 4 and the flash point is 536°F (280°C). The auto ignition is 626°F (330°C). The ball and ring soft point is 305°F (152°C); ASTM E-28-6-7. The peal strength on canvas is 15 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 30 seconds. The delivery rate is 65 seconds for 1 inch x 3 inch cartridge.

Self-extinguishing version of 3748 Adhesive meets UL 94 V-O, UL 1410 requirements.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 5500 cP5500 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1.38 MPa200 psi
Elongation at Break 1850 %1850 %
Adhesive Bond Strength 1.90 MPa
@Temperature 22.2 °C
276 psi
@Temperature 72.0 °F
on Douglas Fir
Impact Test  1.13 J
@Temperature -17.8 °C
0.833 ft-lb
@Temperature 0.000 °F
 5.65 J
@Temperature 22.0 °C
4.17 ft-lb
@Temperature 71.6 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 79.0 °C174 °FHeat Resistance Temp
Flammability, UL94 V-0V-0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE 4445 CV KIT
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray

PMMA08 / 53355

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.