MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 9182A is a medium viscosity, flame retardant epoxy encapsulant. It adheres well to most electronic and aerospace-industry materials like metals, glass, ceramic, industrial laminates and rigid plastics. TRA-CAST 9182A is recommended for potting, laminating, transformer encapsulating, filament winding and coil embedding applications where stress relief matched with fire retardancy is required. TRA-CAST 9182A has an easy mix ratio and is a durable electrical insulator, stable over a wide temperature range.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccCured
Viscosity 35000 cP
@Temperature 25.0 °C
35000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 15.7 kV/mm400 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 90.0 °C
1.00 hour
@Temperature 194 °F
 240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/100Resin/Hardener
Working Life minutes 140

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
3M Jet-melt™ 3748 V-O Light Yellow Adhesive: High-Melt Technology
Dow SE 4445 CV KIT
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
3M FM069 Indoor UL Recognized Brite Silver Polyester Label Products

PTRAC190 / 71118

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.