MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond 240 Cyanoacrylate, gap filling
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines.

Features & Benefits:

  • Rapid development of high strength
  • Ease of use – no mixing or heat cure
  • Bonds most materials
  • 100% reactive, no solvents

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccUncured
Viscosity 1200 - 2500 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 2.00 - 7.00 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ISO 868
Adhesive Bond Strength >= 5.00 MPaPC, Substrate Failure, Shear; ISO 4587
 >= 6.00 MPaABS, Substrate Failure, Shear; ISO 4587
 >= 6.00 MPaPVC, Substrate Failure, Shear; ISO 4587
 8.00 - 9.00 MPaAluminum, Shear; ISO 4587
 10.0 MPaZinc, Shear; ISO 4587
 14.0 MPaPhenolic, Shear; ISO 4587
 21.0 - 25.0 MPaSteel, Shear; ISO 4587
Impact 3.0 - 5.0kJ/m2 Adhesive Impact Strength; ASTM D950
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.5
@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
Thermal Conductivity 0.100 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 20.0 secSteel, handling time
 15.0 - 20.0 secBuna N Rubber, handling time
 15.0 - 20.0 secPhenolic, handling time
 24.0 hourfull strength
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.4
Strength Retention10% at 150°CRelative to 0°C
 100% at 0°CRelative to 0°C
 30% at 100°CRelative to 0°C
 55% at -50°CRelative to 0°C
 90% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERMA858 / 162752

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.