MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond 240 Cyanoacrylate, gap filling
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines.

Features & Benefits:

  • Rapid development of high strength
  • Ease of use – no mixing or heat cure
  • Bonds most materials
  • 100% reactive, no solvents

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Viscosity 1200 - 2500 cP
@Temperature 25.0 °C
1200 - 2500 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C35.6 - 44.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ISO 868
Adhesive Bond Strength >= 5.00 MPa>= 725 psiPC, Substrate Failure, Shear; ISO 4587
 >= 6.00 MPa>= 870 psiABS, Substrate Failure, Shear; ISO 4587
 >= 6.00 MPa>= 870 psiPVC, Substrate Failure, Shear; ISO 4587
 8.00 - 9.00 MPa1160 - 1310 psiAluminum, Shear; ISO 4587
 10.0 MPa1450 psiZinc, Shear; ISO 4587
 14.0 MPa2030 psiPhenolic, Shear; ISO 4587
 21.0 - 25.0 MPa3050 - 3630 psiSteel, Shear; ISO 4587
Impact 3.0 - 5.03.0 - 5.0kJ/m2 Adhesive Impact Strength; ASTM D950
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.5
@Frequency 10000 Hz
2.5
@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm635 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.250 - 0.333 min0.00417 - 0.00556 hourSteel, handling time
 0.250 - 0.333 min0.00417 - 0.00556 hourBuna N Rubber, handling time
 0.250 - 0.333 min0.00417 - 0.00556 hourPhenolic, handling time
 1440 min24.0 hourfull strength
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.4
Strength Retention10% at 150°CRelative to 0°C
 100% at 0°CRelative to 0°C
 30% at 100°CRelative to 0°C
 55% at -50°CRelative to 0°C
 90% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERMA858 / 162752

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.