MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Design/Construction:
Side 1: Cured Rubber
Side 2: Cured Rubber

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness >= 50.8 microns>= 2.00 milSide 1
 >= 50.8 microns>= 2.00 milSide 2
 76.2 microns3.00 milPolyethylene Interleave
 88.9 microns3.50 milPrime Coated 2113 Fiberglass, Substrate
 165 - 216 microns6.50 - 8.50 milOverall
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 5040 - 50Compound Property
Tensile Strength >= 5.52 MPa>= 800 psiCompound Property
Elongation at Break >= 500 %>= 500 %Compound Property
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
UL RTI, Electrical 200 °C392 °Fper UL Card E54153
UL RTI, Mechanical without Impact 220 °C428 °Fper UL Card E54153
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 12.0 Month
@Temperature 21.1 °C
12.0 Month
@Temperature 70.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)7.7 - 9.5
Uncoated Fabric Break Strength195 lb/inWarp Direction, Substrate Property
 75 lb/inFill Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Alcoa QC-10® Aluminum Mold Alloy
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
AISI 1020 Steel, cold rolled
Momentive Performance Materials XE20-A7016U Heat Cured Rubber - Thermal Conductive

PARL225 / 125411

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.