MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories PT-170 Plastic Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  3.85e-7 - 0.000981 GPa
@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.002943 - 0.005886 GPa
@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi
@Temperature 2460 °F,
Time 3.00 hour
 0.0034335 - 0.0063765 GPa
@Temperature 1500 °C,
Time 10800 sec
0.49799 - 0.92485 ksi
@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength  4.90 - 9.81 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
711 - 1420 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 14.7 - 24.5 MPa
@Treatment Temp. 1350 °C,
Time 10800 sec
2130 - 3560 psi
@Treatment Temp. 2460 °F,
Time 3.00 hour
Cold Crushing Strength
 19.6 - 29.4 MPa
@Treatment Temp. 1500 °C,
Time 10800 sec
2840 - 4270 psi
@Treatment Temp. 2730 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.0236 W/m-K
@Temperature 500 °C
7.0921 BTU-in/hr-ft²-°F
@Temperature 932 °F
 1.1399 W/m-K
@Temperature 1000 °C
7.8980 BTU-in/hr-ft²-°F
@Temperature 1830 °F
Maximum Service Temperature, Air 1700 °C3090 °Flimited
Shrinkage  -0.900 %
@Temperature 1500 °C,
Time 10800 sec
-0.900 %
@Temperature 2730 °F,
Time 3.00 hour
 -0.600 %
@Temperature 110 °C,
Time 86400 sec
-0.600 %
@Temperature 230 °F,
Time 24.0 hour
 -0.100 %
@Temperature 1350 °C,
Time 10800 sec
-0.100 %
@Temperature 2460 °F,
Time 3.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 63 %63 %
SiO2 32 %32 %
 
Descriptive Properties
Main ApplicationsVarious furnace
Material Required for Estimating (kg/m3)2,500

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact
Anderman Ceramics EZY 88 Zirconia, 88%, Fully Yttria-Stabilized
Thermal Ceramics K-Shield Felt AG/Min-K Composite
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables

CCHOS254 / 124198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.