MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 1000 ppm
  • Slip: 500 ppm
  • Thermal Stabilizer: Yes
Applications:
  • Coextrusion Films
  • Foams
  • Form Fill and Seal Packaging
  • Freezer Film
  • High Clarity Film
  • Lamination Film
  • Poultry Bag
  • Produce Bags
  • Rice Bags

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccExxonMobil method
Vinyl Acetate Content 5.5 %ExxonMobil Method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 1000 ppm
Slip Level 500 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 190 %ASTM D882
Film Elongation at Break, TD 590 %ASTM D882
Puncture Energy 12.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 160 gASTM D1922
Elmendorf Tear Strength TD 80 gASTM D1922
Dart Drop Test 170 gASTM D1709A
Film Tensile Strength at Break, MD 36000 psiASTM D882
Film Tensile Strength at Break, TD 3500 psiASTM D882
1% Secant Modulus, MD 18000 psiASTM D882
1% Secant Modulus, TD 21000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 216 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM D1003
Gloss 74 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer

PEX99224 / 175460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.