Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. These superior strength properties, along with excellent heat sealing and hot tack performance, make this a very versatile packaging film resin. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications:- Bag in Box
- Barrier Food Packaging
- Blown Film
- Food packaging
- Form Fill and Seal Packaging
- Freezer Film
- Heavy Duty Bags
- Ice Bags
- Lamination Film
- Multilayer Packaging Film
- Stand Up Pouches
Information provided by ExxonMobil |