MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
European Field Elm Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Key Words: Ulmus procera; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.670 g/ccAir Dry (12-15% Moisture Content)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 5000 NSide
Tensile Strength, Ultimate 3.90 MPaPerpendicular to Grain
 78.0 MPaAxial
Modulus of Rupture 0.0870 GPaStatic Bending
Flexural Modulus 10.78 GPaStatic Bending
Compressive Strength 9.80 MPaPerpendicular to Grain
 55.0 MPaParallel to Grain
Shear Strength 6.90 MPaOrientation Unknown
Toughness 23.6 J2 cm x 2 cm sample
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.30 %Axial; Green to Zero Moisture
 4.6 %Radial; Green to Zero Moisture
 8.3 %Tangential; Green to Zero Moisture
 13.8 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Pecan Hickory Wood
European Ash Wood
Hexcel® HexTow® AS4D 12K Standard Modulus Carbon Fiber (12,000 Filaments)
Overview of materials for Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy

PTSE070 / 71316

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.