MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Bayoxide® E AB 21 γ-Fe2O3
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No: 1309-37-1. Bayoxide® E AB 21 is a technical iron oxide used in conventional gas-generation airbag systems where it serves as an oxidizing agent and for scorification of the sodium formed in the gas-generating reaction. Thereby, a controlled unfolding of the airbag can be ensured. The requirements placed on the iron oxide used in this critical safety application are high. Bayoxide® E AB 21 has a low heavy metal content, neutral to slightly alkaline pH and excellent free flowing properties.

Information provided by Lanxess.

Key Words: Gamma Iron Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 1.0 %DIN EN ISO 787-2
Loss On Ignition <= 1.5 %
Particle Size 0.70 µmDIN ISO 13320
pH >= 6.0DIN EN ISO 787-9
Specific Surface Area 22 - 30 m²/gISO 9277
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Monthbulk bags
 60.0 Monthbags
 
Component Elements PropertiesOriginal ValueComments
CaO 0.30 %
Fe2O3 >= 99.5 %γ phase
MgO 0.20 %
MnO 0.30 %
Na2O 0.10 %
SiO2 1.0 %
 
Descriptive Properties
Content<50 mg/kgHeavy metal content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iron (III) Oxide, Fe2O3 (Hematite)
Uranium (IV) Oxide, UO2 (Uraninite)
Limonite (Fe2O3-nH2O)
Iron (III) Oxide, Fe2O3 (Maghemite)
Iron (II, III) Oxide, Fe3O4 (Magnetite)

PLANY8407 / 208800

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.